Grade Description of RSS as per Green Book.

RSS1: The grade must be produced under conditions where all processing operations are carefully and uniformly controlled. Each bale must be packed free of moulds but very slight traces of dry mould on wrappers or bale surfaces adjacent to wrapper found at the time of delivery will not be objected to, provided there is no penetration of mould inside the bale. Oxidized spots or streaks, weak, heated, under cured, and over smoked, opaque and burnt sheets are not permissible.

The rubber must be dry, clean, strong and evenly smoked and free from blemishes, specks, rust, blisters, sand, dirty packing and any other foreign matter. Small pinhead bubbles if scattered, will not be objected to


RSS 2: Slight rust or a slight amount of dry mould on wrappers, bale surfaces and interior sheets, found at the time of delivery, will not be objected to, provided these, either singly or in combination, do not exist in more than 5% of the number of bales included in the delivery, lot or tender as determined by the number of bales inspected. Small bubbles and slight specks of bark, if scattered, will not be objected to.

Oxidized spots or streaks, weak, heated, under cured, and over smoked, opaque and burnt sheets are ruled out. The rubber must be dry, clean strong and free from blemishes, blisters, sand, dirty packing and all other foreign matter other than specified above as permissible.


RSS3: Rust and dry mould on wrappers, bale surfaces and interior sheets, found at the time of delivery, will not be objected to, provided these conditions either singly or in combination do not exist to an objectionable extent on or in more than 10% of the number of bales included in the delivery, lot or tender as determined by the number of bales inspected. Slight blemishes in color, small bubbles and small specks of bark are permissible. The other parameters are the same as for RSS 2


RSS4: Rust, dry mould on wrappers, bale surfaces and interior sheets, found at time of delivery, will not be objected to provide these conditions, either singly or in combination, do not exist to an objectionable extent on or in more than 20% of the number of bales included in the delivery, lot or tender as determined by the number of bales inspected.


RSS5: Rust, dry mould on wrappers, bale surfaces and interior sheets, found at the time of delivery will not be objected to provided these conditions, either singly or in combination, do not exist to an objectionable extent on or in more than 30 % of the number of bales.

Large bark particles, bubbles and small blisters, stains, over smoked, slightly sticky rubber and small blemishes are permissible proved they are not present to a marked degree. Slightly under cured rubber is also permissible but not weak, heated, burnt rubber, and those with oxidized spots or streaks. The rubber must be dry, firm, and free of sand, dirty packing and other foreign matter other than specified above as permissible.

 

 
 
 